Step 4: Filming

Put power enabled tantalum block into Mn(NO3)2 solution, decomposes Mn(NO3)2 into MnO2. Repeat this process many times to fulfill tiny pores of tantalum block.


Step 5: Coating

Cover with graphite and silver on layer MnO2, and solid tantalum capacitor production process finished.


Step 6: Sealing

Pack differ according to differenty type.


Step 7: Aging

Separate and remove defective objects via adding certain voltage and temperature.