Step 1 : Shaping

Shap high purity tantalum powder with tantalum wires into a basic tantalum block.


Step 2: Sintering

Burn tantalum block under high temperature and vacuum condition to make part of it melt.


Step 3: Power enabling

Lay tantalum block into electrolyte, tantalum block connect with anode and electrolyte connected with cathode. Ta2O2 electrolyte film will form on tantalum block surface after applied voltage and current flow over.